Research Article
Tailoring the Curing Kinetics of NBR-Based Rubber Compounds for Additive Manufacturing of Rod Seals
Figure 12
Pre-estimation of scorch behavior of the rubber mixtures and 3D printing. (a) Mooney Scorch measurements of the reference mixture (#1, Batch 4) and both optimized mixtures (#2, #3, Batch 4) at 100°C, (b) torque curve during the 3D printing at 100°C.
(a) |
(b) |