Research Article

Synthesis and Thermal Adsorption Characteristics of Silver-Based Hybrid Nanocomposites for Automotive Friction Material Application

Table 4

Process parameter for silver matrix composites.

DescriptionsPreheating temperatureRotational speed (stir)Impeller typeStir timeFeed rateDie preheat temperatureVacuum pressure
MatrixReinforcements

Units400°C500 rpmGraphite10 min0.9 g/sec350°C bar