Research Article

Development of Durian Rind/Polypyrrole Composite and Its Application in Removing of Anionic Dyes

Table 2

Parameters of applied isotherm models for dye on DR/PPy material (condition: DR/PPy dosage of 1.5 g L-1, contacting time of 23 h, and pH of 5).

DyeTemperature (°C)LangmuirFreundlich

Methyl orange20178.250.24820.98120.0133-0.07460.335051.86790.9825
30191.200.27100.99190.0122-0.06870.391651.29280.9675
40186.920.40350.99300.0082-0.04720.341662.35410.9654
50193.050.40920.99140.0081-0.04660.357563.77360.9749

Sunset yellow20128.210.32160.99880.0103-0.05850.238153.65260.7913
30152.440.32250.98990.0077-0.05840.234759.48890.8012
40161.810.39850.99310.0062-0.04780.255062.50460.8237
50171.230.45950.99170.0054-0.04170.284564.50220.8046

Amaranth20105.370.46610.99840.0071-0.04110.155752.97130.8836
30128.531.22140.99970.0027-0.01610.146672.73480.6463
40133.692.09520.99990.0016-0.00950.154078.79420.8508
50147.712.83260.99990.0012-0.00700.130497.46660.9373