Research Article

Removal of Pb(II) from Aqueous Solutions with Manganese Oxide-Modified Diatomite

Figure 2

SEM images of Mn/diatomite samples prepared at different KMnO4/HCl molar ratios: (a, b) 1 : 1; (c, d) 1 : 2; (e, f) 1 : 4 (experimental conditions: hydrothermal time and temperature are 16 h and 80°C, respectively).
(a)
(b)
(c)
(d)
(e)
(f)