Research Article
[Retracted] Processing and Characterization of Novel Bio-Waste Hybrid Brick Composites for Pollution Control
Table 2
Composites fabrication detail.
| Condition | Process |
| Mixing condition | The materials used are as follows: coconut waste fibre, wood, wheat straw, animal drugs, sand, cement, and gypsum. | Coconut waste fibre, wood, wheat straw, and animal dung were mixed for the first ten mins | After that, cement, sand, and water were mixed with the ingredients and mixed for another ten minutes. |
| Moulding conditions | The mixed material was poured into the mould and levelled, and kept in the mould for two days. |
| Dry condition | The newly developed bricks were held in the environmental atmosphere, and water was provided daily to avoid the cracks and increase the strength | After 6 days, the developed bricks were put in the muffle furnace at 60°c to remove the moisture for 8 hours. |
|
|