Research Article
[Retracted] Process Optimization for Development of Guar Gum-Based Biodegradable Hydrogel Film Using Response Surface Methodology
Figure 5
(a) Combined effects of initiator and crosslinker on transparency at the optimum value of plasticizer concentration (2.88 mL/100 mL GS). (b) Combined effects of initiator and plasticizer concentration on transparency at the optimum value of crosslinker (0.02 mg/100 mL GS).