Research Article
[Retracted] Process Optimization for Development of Guar Gum-Based Biodegradable Hydrogel Film Using Response Surface Methodology
Table 3
Experimental results of response for the development of hydrogel film.
| Expt. no | Independent parameters | Responses | Initiator (mg/100 mL GS) | Cross linker (mg/100 mL GS) | Plasticizer (mL/100 mL GS) | Biodegradation (% wt. loss) | Color difference (ΔE) | Hardness (N) | Swelling index (%) | Transparency (per mm thickness) % |
| 1 | 0.15 | 0.05 | 2 | 14.90 | 3.97 | 116.8 | 191.46 | 61.3 | 2 | 0.1 | 0.05 | 4 | 13.91 | 6.99 | 129.1 | 125.36 | 58 | 3 | 0.1 | 0.05 | 4 | 12.84 | 7.54 | 129.5 | 110.56 | 59.4 | 4 | 0.1 | 0.02 | 6 | 4.79 | 6.73 | 127.25 | 120.94 | 56.2 | 5 | 0.1 | 0.02 | 2 | 9.84 | 10.29 | 126.65 | 187.23 | 49.3 | 6 | 0.1 | 0.08 | 2 | 4.32 | 5.41 | 103.75 | 132.01 | 56.3 | 7 | 0.05 | 0.05 | 6 | 13.44 | 10.57 | 128.5 | 139.71 | 39.4 | 8 | 0.1 | 0.05 | 4 | 11.54 | 7.45 | 130.85 | 121.45 | 59.8 | 9 | 0.05 | 0.02 | 4 | 7.79 | 25.65 | 128 | 151.08 | 19.3 | 10 | 0.1 | 0.05 | 4 | 12.41 | 7.32 | 129.5 | 110.56 | 58.4 | 11 | 0.05 | 0.05 | 2 | 6.04 | 25.10 | 111.45 | 89.70 | 26.6 | 12 | 0.1 | 0.08 | 6 | 5.83 | 7.62 | 129.2 | 141.89 | 65.8 | 13 | 0.1 | 0.05 | 4 | 13.36 | 6.99 | 129.95 | 119.65 | 58.6 | 14 | 0.05 | 0.08 | 4 | 18.34 | 14.29 | 106.85 | 110.56 | 40.6 | 15 | 0.15 | 0.05 | 6 | 8.49 | 15.39 | 128 | 131.86 | 62 | 16 | 0.15 | 0.08 | 4 | 7.63 | 15.65 | 123.35 | 161.91 | 59.9 | 17 | 0.15 | 0.02 | 4 | 22.13 | 8.516 | 122.05 | 213.3 | 56.9 |
|
|
, indicates the maximum and minimum values. |