The firing cycle of all-porcelain mini-dumbbell specimens.

PorcelainPredrying Heating-upEnd firingVacuum
build-up (°C) (min) (min)(°C/min) (°C) (min)(min)

1st firing6006.006.00559301.006.00
2nd firing6006.006.00539201.006.00
3rd firing6006.006.00519101.006.00