Research Article
An Evaluation of the Gap Sizes of 3-Unit Fixed Dental Prostheses Milled from Sintering Metal Blocks
Table 3
Mean ± standard deviation of each point of gap for two groups with results of the Mann-Whitney test (unit: μm).
| Points | | Premolar | Molar | SMB | LWC | value | SMB | LWC | value |
| 1 | 10 | 62.0 ± 22.7 | 59.4 ± 10.7 | 0.880 | 75.7 ± 36.8 | 98.0 ± 14.9 | 0.151 | 2 | 10 | 39.3 ± 17.6 | 55.6 ± 17.6 | 0.045 | 41.1 ± 15.0 | 48.7 ± 10.8 | 0.112 | 3 | 10 | 104.5 ± 21.0 | 79.3 ± 14.6 | 0.005 | 113.7 ± 20.1 | 82.7 ± 24.5 | 0.008 | 4 | 10 | 97.2 ± 17.8 | 79.0 ± 11.1 | 0.028 | 116.3 ± 20.0 | 75.8 ± 28.8 | 0.007 | 5 | 10 | 36.0 ± 12.3 | 50.0 ± 6.3 | 0.019 | 34.8 ± 8.3 | 59.0 ± 7.6 | 0.001 | 6 | 10 | 55.6 ± 21.3 | 68.1 ± 11.1 | 0.131 | 60.1 ± 29.1 | 76.2 ± 20.0 | 0.059 | 7 | 10 | 58.3 ± 22.0 | 71.4 ± 11.8 | 0.096 | 101.4 ± 36.0 | 74.2 ± 24.3 | 0.096 | 8 | 10 | 39.3 ± 15.1 | 62.3 ± 14.5 | 0.005 | 52.4 ± 12.0 | 52.0 ± 12.1 | 0.940 | 9 | 10 | 109.0 ± 36.2 | 86.6 ± 14.2 | 0.082 | 119.2 ± 29.1 | 83.4 ± 26.9 | 0.016 | 10 | 10 | 116.0 ± 33.6 | 90.2 ± 12.0 | 0.007 | 100.2 ± 17.3 | 102.7 ± 20.4 | 0.597 | 11 | 10 | 44.2 ± 11.4 | 63.6 ± 12.7 | 0.003 | 53.8 ± 17.2 | 51.3 ± 12.6 | 0.705 | 12 | 10 | 62.5 ± 22.6 | 70.0 ± 12.0 | 0.406 | 68.8 ± 28.5 | 83.4 ± 22.7 | 0.257 |
| Total | 120 | 68.6 ± 35.6 | 69.6 ± 16.9 | 0.139 | 78.1 ± 37.4 | 73.9 ± 25.6 | 0.852 |
|
|
SMB: sintering metal block (experimental group); LWC: lost-wax technique + casting (gold standard group). The results of Mann-Whitney test.
|