The density, grain size, and crystalline phase structure of zirconia.
| Group | Density (g/cm3) | Relative density (%) | Grain size (μm) | Crystalline phase structure | Young’s modulus (GPa) | Mean | SD | Mean | SD | Mean | SD |
| DLP | 6.0198 | 0.0213 | 99.0099 | 0.6030 | 0.0326 | Tetragonal | 221.4 | 2.2 | MILL | 6.0382 | 0.0115 | 99.3125 | 0.5911 | 0.0330 | Tetragonal | 225.1 | 3.4 |
|
|