Research Article

Effect of Veneering and Hydrothermal Aging on the Translucency of Newly Introduced Extra Translucent and High Translucent Zirconia with Different Thicknesses

Table 3

Difference between TP values of specimens before and after aging.

ThicknessXTVXTHTVHT

0.5-4.39 (0.67)A,b-3.37 (0.49)B,f
; 1-2.96 (1.92)C,a-3.36 (0.99)C,c-1.97 (0.87)C,e-2.60 (0.43)C,g
; 1.5-2.20 (1.02)DE,a-2.58 (0.76)D,cd-1.47 (0.96)E,e-2.01 (0.43)DE,h
; 2-1.83 (1.94)F,a-2.02 (0.22)F,d-1.16 (0.73)F,e-1.63 (0.39)F,h

Same superscript uppercase letters indicate no statistically significant difference within each row. Same superscript lowercase letters indicate no statistically significant difference within each column ().