Chemical composition, sintering conditions, and manufacturer of materials.

MaterialCompositionSintering temperature/timeManufacturer

VITA YZ XT (preshaded+nonshaded)ZrO2 (86-91%)
Y2O3 (8-10%)
HfO2 (1-3%)
Al2O3 (0-1%)
Pigments (0-1%)
1450°C/7 hoursVITA Zahnfabrik, Germany
VITA YZ ST (preshaded+nonshaded)ZrO2 (88-93%)
Y2O3 (6-8%)
HfO2 (1-3%)
Al2O3 (0-1%)
Pigments (0-1%)
1530°C/4 hoursVITA Zahnfabrik, Germany
VITA YZ HT (preshaded+nonshaded)ZrO2 (90-95%)
Y2O3 (4-6%)
HfO2 (1-3%)
Al2O3 (0-1%)
Pigments (0-1%)
1450°C/10 hoursVITA Zahnfabrik, Germany