(a) The results of HE staining of cartilage before alloy implantation and 2, 4, and 8 weeks after implantation. (b) The IHC results of LC3-II in cartilage in the Fe-30Mn-0.6N alloy group and the Ti-6Al-4V alloy group before implantation and 2 and 4 weeks after implantation. (c) Analysis results of MOD of LC3-II expression in the Fe-30Mn-0.6N alloy group and the Ti-6Al-4V alloy group. .