Research Article

Adhesive Ability of Different Oral Pathogens to Various Dental Materials: An In Vitro Study

Table 5

Actinomyces viscosus group (plate colony counting).

2 h4 h6 h8 h12 h16 h20 h24 h

3M Z350 resin0.08 ± 0.040.69 ± 0.151.93 ± 0.562.19 ± 1.023.92 ± 0.426.71 ± 0.607.38 ± 1.119.25 ± 0.55
Glass ionomer cement0.02 ± 0.010.33 ± 0.171.03 ± 0.181.53 ± 0.443.26 ± 0.643.17 ± 0.233.95 ± 0.625.81 ± 0.16
Icon0.01 ± 0.000.03 ± 0.010.34 ± 0.090.34 ± 0.060.57 ± 0.250.68 ± 0.201.83 ± 0.085.93 ± 0.90

The experimental results were expressed as mean ± standard deviation (unit: ×106 CFU/ml).