Research Article
Systematic Monitoring and Evaluating the Wear of Alumina Wheel When Grinding the Workpiece of Cr12
Figure 5
The surface morphology with different cumulative material removal. (a) V′ = 20 mm3/mm, (b) V′ = 60 mm3/mm, (c) V′ = 140 mm3/mm, (d) V′ = 210 mm3/mm, and (e) V′ = 290 mm3/mm.
(a) |
(b) |
(c) |
(d) |
(e) |