The Effects of Adding Elements of Zinc and Magnesium on Ag-Cu Eutectic Alloy for Warming Acupuncture

Figure 8

MC3T3-E1 cell morphology for 2 days by elution (s) standard (negative control): (a) Ag65-Cu30-Zn5, (b) Cu70-Ag30, (c) Ag68-Cu30-Mg2, (d) phosphor bronze, (e) Ti-6Al-4V alloy, and (f) STS304.