Research Article
The Effects of Adding Elements of Zinc and Magnesium on Ag-Cu Eutectic Alloy for Warming Acupuncture
Table 1
Results of composition, drawing diameter, and straightness.
| Materials | Ag (wt%) | Cu (wt%) | Zn (wt%) | Mg (wt%) | Drawing process (diameter, mm) | Straightness (gap length, mm) |
| Ag80 | 80 | 20 | | | 0.5 | Broken wire | Ag72 | 72 | 28 | | | 3 | Broken wire | Ag70 | 70 | 30 | | | 0.4 | | Ag60 | 60 | 40 | | | 4.5 | Broken wire | Ag40 | 40 | 60 | | | 0.7 | Broken wire | Ag30 | 30 | 70 | | | 0.4 | | Ag20 | 20 | 80 | | | 0.8 | Broken wire | Ag65-Cu30-Zn5 | 65 | 30 | 5 | | 0.4 | | Ag68-Cu30-Mg2 | 68 | 30 | | 2 | 0.4 | |
|
|