Research Article
Laboratory Leaching Tests to Investigate Mobilisation and Recovery of Metals from Geothermal Reservoirs
Figure 12
Concentration (in ppb) of the “at risk” elements in HTLMix reacted with the mixture of 0.1 M HCl and 0.03 M HNO3 at 100°C and 200°C temperature under 200 bar pressure in Ti batch reactors after 770 hours and 530 hours, respectively (absence of data points reflects concentrations below the limits of detection).