Statistics of the average value of debris of two particle sizes for dry and water-saturated coal samples after impact loading.
| | (0~0.2 mm, dry, ) | (0.2~5 mm, dry, ) | (0~0.2 mm, saturated, ) | (0.2~5 mm, saturated, ) | (%) | (%) |
| 0° | 0.653 | 10.551 | 0.4489 | 5.007 | 31.2557 | 52.54478 | 22.5° | 0.617 | 9.004 | 0.4878 | 5.968 | 20.94003 | 33.71835 | 45° | 0.593 | 8.97 | 0.602 | 9.183 | -1.517707 | -2.3746 | 67.5° | 0.776 | 11.879 | 0.54 | 5.579 | 30.41237 | 53.03477 | 90° | 0.589 | 7.4189 | 0.506 | 3.533 | 14.09168 | 52.37838 |
|
|