Research Article
Study on Mechanical Properties of PET Fiber-Reinforced Coal Gangue Fine Aggregate Concrete
| Specimen | Replacement rate (%) | Cement (kg·m-3) | Water (kg m-3) | Coarse aggregate (kg·m-3) | Fine aggregate | Water reducer (kg·m-3) | River sand (kg·m-3) | Coal gangue (kg·m-3) |
| CGC-0 | 0 | 379.6 | 205 | 1151.31 | 619.9 | 0 | 1.63 | CGC-1 | 10 | 379.6 | 205 | 1151.31 | 619.9 | 59.56 | 1.63 | CGC-2 | 20 | 379.6 | 205 | 1151.31 | 619.9 | 119.13 | 1.63 | CGC-3 | 30 | 379.6 | 205 | 1151.31 | 619.9 | 178.69 | 1.63 | CGC-4 | 40 | 379.6 | 205 | 1151.31 | 619.9 | 238.25 | 1.63 | CGC-5 | 50 | 379.6 | 205 | 1151.31 | 619.9 | 297.81 | 1.63 |
|
|