Research Article
Effects of Water Immersion on the Long-Term Bearing Characteristics of Crushed Gangue in Goaf
Table 4
Grain size distribution and fractal dimensions of crushed sandstone samples of different axial stresses before and after compression.
| Axial stress | State | Quality (kg) | | | 0~10 mm | 10~20 mm | 20~30 mm | 30~40 mm | 40~50 mm | 50~60 mm |
| 1.50 MPa | Before compression | 25.31 | 10.48 | 8.05 | 6.78 | 5.98 | 5.40 | 2.5000 | 0.0531 | After compression | 26.83 | 11.05 | 7.71 | 6.04 | 5.88 | 4.49 | 2.5531 | 3.50 MPa | Before compression | 25.31 | 10.48 | 8.05 | 6.78 | 5.98 | 5.40 | 2.5000 | 0.0914 | After compression | 29.68 | 10.16 | 6.98 | 5.37 | 5.32 | 4.50 | 2.5914 | 5.50 MPa | Before compression | 25.31 | 10.48 | 8.05 | 6.78 | 5.98 | 5.40 | 2.5000 | 0.1184 | After compression | 31.85 | 6.86 | 7.32 | 6.72 | 5.14 | 4.11 | 2.6184 | 7.50 MPa | Before compression | 25.31 | 10.48 | 8.05 | 6.78 | 5.98 | 5.40 | 2.5000 | 0.1481 | After compression | 33.07 | 8.73 | 6.12 | 5.57 | 4.73 | 3.78 | 2.6481 |
|
|