Table 4
Cementation failure number of sample model at different temperatures.
Serial number
Initial temperature (°C)
Termination temperature (°C)
Cementation failure numbers (piece)
1#
20
50
720
2#
20
90
874
3#
20
120
1148
4#
20
130
1041
5#
20
150
998