Research Article
Development of Modified Grouting Material and Its Application in Roadway Repair Engineering
| | Serial number | Project | Parameters |
| | 1 | Grouting materials | Modified grouting material | | 2 | Water cement ratio | 1.5 : 1 | | 3 | Lag grouting time | 3-5 days after shotcreting | | 4 | Grouting pipe | R25N self-drilling grouting anchor with length of 2.5 m and yield strength of 150 kN | | 5 | Grouting pressure | 2.0-3.0 MPa | | 6 | Grouting quantity | Stop grouting when the design grouting pressure is reached or a large amount of grout leakage occurs | | 7 | Slurry diffusion radius | About 2.5 m | | 8 | Depth of grouting hole | 3.0 m |
|
|