Research Article

Effects of Coarse and Fine Crushed Clay Brick Content on the Compressive Strength of Recycled Aggregate Concrete and the Microscopic Mechanism

Figure 8

Microscopic morphology of NAC and RAC with 0% or 60% coarse crushed clay bricks at the age of 7 d (magnified 3000 times).
(a) 7 d NAC
(b) 7 d RAC with 0% crushed clay bricks
(c) 7 d RAC with 60% coarse crushed clay bricks