Research Article
Effects of Coarse and Fine Crushed Clay Brick Content on the Compressive Strength of Recycled Aggregate Concrete and the Microscopic Mechanism
Table 1
Properties of RAC aggregates and crushed clay bricks used in the tests.
| Test indexes | RAC aggregate | Crushed clay bricks | 0-4.75 mm | 4.75-9.50 mm | 9.50-19 mm | 0-4.75 mm | 4.75-9.50 mm | 9.50-19 mm |
| Apparent density/(g∙cm−3) | 2.60 | 2.65 | 2.61 | 2.30 | 2.43 | 2.41 | Water absorption/(%) | 8.20 | 4.58 | 3.43 | 11.30 | 11.55 | 10.72 | Flat and elongated particles/(%) | — | 7.7 | 6.8 | — | 7.6 | 7.8 | Crushing strength/(%) | — | 23.6 | — | 29.3 | Liquid limit/(%) | 27.3 | — | 27.8 | — | Plastic limit/(%) | 22.2 | — | 23.4 | — | <0.075 mm/(%) | 2.7 | — | 3.5 | — |
|
|