Research Article

Investigation on the Mechanical Properties and Microscopic Characteristics of Modified Steel Slag Concrete under Sulfate Erosion

Table 2

Sieve results of steel slag aggregate.

Mesh diameter (mm)2.364.759.519

Cumulative screen residual (%)98.2196.1363.841.89
Specification grading range (mm)95-10090-10040-800-10