Comparison of Mechanical Properties and Sensitivity of Compressive and Flexural Strength of Artificial Frozen Sand
Table 3
Percentage of the increase in mechanical properties of artificial frozen sand at different curing temperatures.
| Moisture content (%) | Increased percentage of compressive strength in different intervals (%) | Percentage increase of flexural strength in different intervals (%) | Curing temperature −10°C to −15°C | Curing temperature −15°C to −20°C | Curing temperature −10°C to −15°C | Curing temperature −15°C to −20°C |
| 12 | 12.6 | 18.8 | 40.5 | 26.4 | 15 | 24.9 | 57.1 | 134.2 | 49.9 | 18 | 34.5 | 31.0 | 70.4 | 33.1 |
|
|