Research Article
A Study of Dynamic Loading and Unloading Damage of Fiber-Reinforced Concrete under Confining Pressure
Table 4
Measured permeability of C50S1.2-1 test block in cyclic loading and unloading test.
| Axial load (MPa) | Cycle 1 | Cycle 2 | Cycle 3 | Cycle 4 | Measured value of permeability (e − 16 m2) |
| 1 | 2.66 | 8.17 | 10 | 13 | 5 | 7.15 | 9 | 13 | 15 | 10 | 11.34 | 13 | 16 | 18 | 15 | 21.48 | 24 | 26 | 28 | 20 | 28.35 | 31 | 35 | 39 | 15 | 22 | 25 | 28 | 31 | 10 | 17.68 | 19 | 22 | 25 | 5 | 10.24 | 13 | 15 | 17 | 1 | 8.17 | 10 | 13 | 16 |
|
|