Research Article
Effect of Moisture on the Macro Failure Characteristics of Weakly Consolidated Mudstone: Mesomechanism
Table 1
Basic test information of mudstone specimen before and after humidification curing.
| Items | Dry | Moist | N-1 | N-2 | N-3 | Average | M-1 | M-2 | M-3 | Average | Before | After | Before | After | Before | After | Before | After |
| Length (mm) | 100.13 | 100.12 | 99.94 | 100.06 | 100.36 | 100.37 | 100.33 | 100.33 | 100.38 | 100.4 | 100.36 | 100.36 | Diameter (mm) | 50.02 | 50.15 | 50.04 | 50.07 | 49.91 | 49.93 | 50.07 | 50.07 | 50.08 | 50.09 | 50.02 | 50.03 | Weight (g) | 400.25 | 404.17 | 410.23 | 404.88 | 391.15 | 396.12 | 418.72 | 423.58 | 406.23 | 411.18 | 405.37 | 410.29 | RMC (%) | 0 | 0 | 0 | 0 | 1.27 | 1.16 | 1.21 | ā1.20 | UCS (MPa) | 9.04 | 13.39 | 11.88 | 11.44 | 6.625 | 8.24 | 6.78 | 7.215 | (GPa) | 6.82 | 15.68 | 13.63 | 12.04 | 5.675 | 8.11 | 5.73 | 6.505 |
|
|