Research Article
Effect of Chromium Ion on the Strength Characteristics and Damage Law of Red Clay
Figure 9
Comparison curves of damage variables under different confining pressures. (a) The initial dry density is 1.45 g/cm3. Concentration of Cr3+ 0%. (b) The initial dry density is 1.45 g/cm3. Concentration of Cr3+ 0.1%.
(a) |