Effect of Chromium Ion on the Strength Characteristics and Damage Law of Red Clay
Table 7
Hyperbolic fitting parameter table of different dry densities and confining pressures of 300 kPa (
, ).
| Dry density (g/cm3) | Chromium ion concentration (%) | | | | | |
| 1.35 | 0 | 1.410 | 0.550 | 70.922 | 181.818 | 0.989 | 0.01 | 1.645 | 0.660 | 60.789 | 151.515 | 0.987 | 0.05 | 2.814 | 0.890 | 35.534 | 25.252 | 0.969 | 0.1 | 3.996 | 1.270 | 25.024 | 21.978 | 0.973 | 1.40 | 0 | 0.655 | 0.280 | 152.74 | 357.143 | 0.981 | 0.01 | 0.889 | 0.410 | 112.465 | 243.902 | 0.985 | 0.05 | 1.322 | 0.620 | 75.645 | 161.29 | 0.976 | 0.1 | 2.707 | 0.820 | 36.942 | 121.951 | 0.977 | 1.45 | 0 | 0.430 | 0.290 | 232.558 | 344.828 | 0.993 | 0.01 | 0.698 | 0.340 | 143.21 | 294.118 | 0.985 | 0.05 | 0.890 | 0.350 | 112.36 | 285.714 | 0.991 | 0.1 | 1.076 | 0.410 | 92.923 | 243.902 | 0.981 |
|
|