Mechanical parameters of the “filling body-remaining coal pillar” structure.

LithologyCompressive strength (σh)/MPaDensity (ρ)/kN·m-3Elastic modulus ()/GPaPoisson’s ratio (μ)Cohesion ()/MPaInternal friction angle (φ)/°Width ()/mWidth ()/m

Filling body502456110.223.334410~22
Filling body4024569.30.222.954010~22
Filling body3024565.90.232.653710~22
Coal pillar814400.9820.231.72815~ 3