Research Article

Experimental Study of Seepage Characteristics of Filling Structures in Deep Roadway

Table 5

Statistics of sand production in each bottle.

Test numberSeepage pressure loading rateKaolin contentLoss amounts of sandy-clay mixtureTotal amounts of sandy-clay mixture
1 min2 min3 min4 min5 min6 min7 min8 min
MPa/min%gg

10.01306.517.843.014.98.65.24.23.9104.1
20.08308.425.661.015.76.56.64.82.4131.0
30.01203.415.741.46.85.13.02.0/77.4
40.08202.514.054.99.68.37.93.2/100.4
50.01100.116.010.02.01.00.1//29.2
60.08100.124.225.011.07.02.0//69.3