Research Article
Study on Spontaneous Combustion Law and Prevention Technology of Abandoned Coal in Goaf of Coal Mine
Table 1
The test coal sample selection and coal sample numbers.
| | No. | Coal seam | Coal mine | Remarks |
| | No. 1 | Layer 4# | Jiudaoling Coal Mine in Liaoning Province | Coal seams are prone to spontaneous combustion. They are used as reference coal samples for this study. Long flame coal (bituminous coal) | | No. 2 | Layer 8#-1 | Changping Coal Mine of Shanxi Jinmei Group 84301 working face of Fushan well | Spontaneous coal seam (class II), the metamorphism belongs to lean coal—anthracite stage | | No. 3 | Layer 8#-2 | | No. 5 | Layer 15# | 150405 working face in Duanwang Coal Mine in Shanxi Province | Spontaneous coal seam (class II). Lean coal (bituminous coal) | | No. 6 | Layer 8+9# | 090506 working face in Duanwang Coal Mine in Shanxi Province | Spontaneous coal seam (class II). Between spontaneous combustion and nonspontaneous combustion. Lean coal (bituminous coal) | | No. 8 | Layer 11# | Duanwang Coal Mine in Shanxi Province | Unworkable seam, drill hole sampling | | No. 9 | Layer 13# | | No. 89 | Layer11# and 13# | Duanwang Coal Mine in Shanxi Province | Unworkable seam, drill hole sampling |
|
|