Permeability test results of samples.
| (MPa) | Permeability (×10-3 μm2) | Smooth fracture | Rough fracture | Matrix | 1# | 2# | 3# | 4# | 5# | 6# | 7# |
| 2 | 241.42 | 1921.01 | 2418.00 | 3350.00 | 263.21 | 1413.00 | 0.187 | 5 | 180.62 | 1737.92 | 2290.00 | 3158.00 | 166.41 | 1181.25 | 0.165 | 9 | 148.06 | 1586.46 | 2032.00 | 3053.00 | 94.10 | 756.78 | 0.122 | 15 | 61.63 | 1222.27 | 1874.54 | 2942.00 | 41.63 | 473.13 | 0.083 | 20 | 35.41 | 999.94 | 1660.93 | 2805.00 | 12.00 | 283.69 | 0.062 | 25 | 23.04 | 876.56 | 1484.89 | 2681.00 | 6.20 | 201.61 | 0.051 | 30 | 19.91 | 790.13 | 1335.55 | 2618.00 | 3.74 | 96.26 | 0.042 |
|
|