Prediction of High-Cycle Fatigue Performance of 1Cr11Ni2W2MoV Stainless Steel Plate after Foreign Object Damage
Table 2
HCF limit of notched specimens.
| No. | Diameter (mm) | (mm) | (mm) | (mm) | (MPa) |
| 1 | 2 | 1.69 | 0.96 | 0.43 | 615 | 2 | 2 | 1.66 | 0.79 | 0.5 | 776 | 3 | 3 | 2.77 | 1.34 | 0.82 | 667 | 4 | 3 | 2.5 | 1.31 | 0.99 | 658 | 5 | 3 | 2.87 | 1.56 | 1.04 | 637 | 6 | 3 | 2.65 | 1.21 | 1.26 | 610 | 7 | 3 | 2.52 | 0.96 | 1.11 | 761 | 8 | 3 | 2.77 | 1.34 | 1.39 | 599 | 9 | 3 | 2.54 | 1.19 | 1.49 | 600 | 10 | 3 | 2.57 | 1.11 | 1.22 | 814 | 11 | 4 | 3.54 | 1.69 | 1.94 | 507 | 12 | 4 | 2.85 | 1.06 | 1.61 | 607 | 13 | 4 | 3.41 | 1.6 | 1.56 | 567 |
|
|
|