AS4-VRM34 material properties (stack properties) [
6].
| Engineering constant | (MPa) | (MPa) | (MPa) | | | | (MPa) | (MPa) | (MPa) | (t/mm3) | Numerical value | 67,154.93 | 33,542.99 | 34,956.42 | 0.4 | 0.4 | 0.095 | 16,340.57 | 16,340.57 | 5515.81 | |
|
|