Research Article

Development of Decellularized Fish Skin Scaffold Decorated with Biosynthesized Silver Nanoparticles for Accelerated Burn Wound Healing

Figure 7

Percentage weight loss of the DFS scaffold during in vitro degradation at 37°C in PBS solution maintained at pH 7.4. The degradation rate was measured as weight lost by the scaffold per day.