Research Article
Development of Decellularized Fish Skin Scaffold Decorated with Biosynthesized Silver Nanoparticles for Accelerated Burn Wound Healing
Figure 9
Moisture content of DFS scaffold. The moisture content of DFS scaffold was found to be 81.7 ± 3.6%. The graph is presented as the amount of moisture in % present per identical sample (N = 3). The result is expressed as grams of water in 100 g of dry sample weight. Error bars are the standard deviation from triplicate measurements.