Research Article

The Corrosion Performance of Galvanized Steel in Closed Rusty Seawater

Figure 11

SEM images of galvanized steel immersed in CRS solution under different temperatures in 0.1 MPa after 14 days, (a) 273 K; (b) 293 K; (c) 313 K; (d) 333 K.
267353.fig.0011a
(a)
267353.fig.0011b
(b)
267353.fig.0011c
(c)
267353.fig.0011d