Research Article
Hot Corrosion of SrTiO3 Perovskite in Na2SO4 + 50 wt.% V2O5 and Na2SO4 + 10 wt.% NaCl Environments at 900°C
Figure 2
Macroscopic view of SrTiO3 surface, (a) before exposure to hot corrosion and after exposure to (b) Na2SO4 + 50 wt.% V2O5 environment and (c) Na2SO4 + 10 wt.% NaCl environment at 900°C.