Investigation of Corrosion Protection of Austenitic Stainless Steel in 5.5 M Polluted Phosphoric Acid Using 5-Azidomethyl-7-morpholinomethyl-8-hydroxyquinoline as an Ecofriendly Inhibitor
Figure 5
Anodic cyclic potentiodynamic polarization of AISI 321 in 5.5 M polluted phosphoric acid at 20°C after 1 hour of immersion and a general view of the surface state. Arrows indicate the direction of the scan.