Research Article

Investigation of Corrosion Protection of Austenitic Stainless Steel in 5.5 M Polluted Phosphoric Acid Using 5-Azidomethyl-7-morpholinomethyl-8-hydroxyquinoline as an Ecofriendly Inhibitor

Table 2

Thickness loss values and corresponding efficiencies deduced from hydrogen evolution tests.

Inhibitor concentration (mmol/L)Thickness loss (mm/year)Efficiency (%)

Blank2.2
0.50.7565.7
10.5873.5
2.50.3185.9
50.0597.6