Research Article

Immobilization of Lead and Nickel Ions from Polluted Yam Peels Biomass Using Cement-Based Solidification/Stabilization Technique

Table 6

Leaching test results.

Brick compositionLeachate (ppm)Environmental policy

5% YP-Pb(II)0.0820.5
10% YP-Pb(II)0.1450.5
5% YP-Pb(II), replica0.0540.5
10% YP-Pb(II), replica0.1550.5
5% YP-Ni(II)0.2012
10% YP-Ni(II)0.2682
5% YP-Ni(II), replica0.2412
10% YP-Ni(II), replica0.3072