Research Article
Electrochemical Analysis of Ultrathin Polythiolsiloxane Films for Surface Biomodification
Figure 4
Cyclic voltammetry measurements on PMPMS layers crosslinked for 17 hours with 1 mM (a) BMH and (b) BMDPM in DMF. The cured layers were immersed in 80°C deionized water for the indicated time, after which they were immersed in K3Fe(CN)6 solution for the CV measurements. PMPMS deposition: 10 mM PMPMS in DMF, 2 h. Data for an uncrosslinked PMPMS layer are shown in (c).
(a) |
(b) |
(c) |