Research Article

Influence of Hydrogen on Vintage Polyethylene Pipes: Slow Crack Growth Performance and Material Properties

Figure 2

The fracture surface of PE80 sample with no exposure to hydrogen tested at  MPa (m0.5): (a) indication of different zones using optical microscopy and (b) the indication of the first three striations using SEM observation.