Revealing the Impact of High Current Overcharge/Overdischarge on the Thermal Safety of Degraded Li-Ion Batteries

Table 2

Test procedures settings.

Test typeTest procedures

Reference performance test (25°C)(1) Constant current (CC) charging to 4.2 V under 1/3C and then constant voltage (CV) charging under 4.2 V until current decreased to <1/20C
(2) Rest for 30 mins
(3) Discharging to 2.5 V at 1/3C
(4) Rest for 30 mins
Note: The reference performance test lasts for three cycles.

2C cycling at 25°C(1) Constant current (CC) charging to 4.2 V under 2C and then constant voltage (CV) charging under 4.2 V until current decreased to <1/20C
(2) Rest for 30 mins
(3) Discharging to 2.5 V at 2C
(4) Rest for 30 mins