Research Article
Green Hydrogen Production Directly from Seawater with No Corrosion Using a Nonmetallic Electrode: A Novel Solution and a Proof of Concept
Table 1
Dimensions, porosity, and permeability for the nonmetallic rock sample electrodes.
| | Sample no. | Sample diameter (mm) | Sample length (mm) | Porosity (%) | Permeability (md) |
| | 1 | 25.18 | 74.04 | 28.99% | 804.75 | | 2 | 25.09 | 76.56 | 25.07% | 43.57 | | 3 | 25.08 | 75.02 | 21.48% | 61.85 | | 4 | 25.04 | 74.56 | 27.07% | 529.93 | | 5 | 37.74 | 71.83 | 24.14% | 428.42 | | 6 | 37.73 | 73.22 | 23.63% | 182.42 | | 7 | 37.74 | 74.46 | 20.65% | 216.84 |
|
|