Research Article
Green Hydrogen Production Directly from Seawater with No Corrosion Using a Nonmetallic Electrode: A Novel Solution and a Proof of Concept
Table 2
Calculated pore volume for the nonmetallic rock sample electrodes.
| Sample no. | Sample diameter (mm) | Sample length (mm) | Porosity (%) | Pore volume cubic centimeter |
| 3 | 25.08 | 75.02 | 21.48% | 7.96 | 2 | 25.09 | 76.56 | 25.07% | 9.49 | 4 | 25.04 | 74.56 | 27.07% | 9.94 | 1 | 25.18 | 74.04 | 28.99% | 10.69 | 7 | 37.74 | 74.46 | 20.65% | 17.20 | 6 | 37.73 | 73.22 | 23.63% | 19.34 | 5 | 37.74 | 71.83 | 24.14% | 19.40 |
|
|