Research Article
Effects of Gas-Diffusion Layers and Water Management on the Carbon Corrosion of a Catalyst Layer in Proton-Exchange Membrane Fuel Cells
Figure 5
Electrochemical performance of MEA with both GDL A and GDL B before and after 3000 cycles of AST. (a) Polarization curve, (b) galvanostatic EIS at 1.0 A cm-2, (c) CVs, (d) ECSA change of MEA, and comparison of the degradation effect between the modified protocol and DOE AST protocol using CV: (e) MEA with GDL A and (f) MEA with GDL B.
| (a) |
| (b) |
| (c) |
| (d) |
| (e) |
| (f) |